MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in general.

Data provided by the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.296 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 33 - 42
Tensile Strength, Ultimate 170000 - 210000 psi
Elongation at Break 7.0 - 20 %
Tensile Modulus 207 GPa
Poissons Ratio 0.31
Shear Modulus 76.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000424 ohm-cm
Curie Temperature <= 95.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 21.0 - 100 °C
Mean
 14.0 µm/m-°C
@Temperature 21.0 - 300 °C
Mean
 14.7 µm/m-°C
@Temperature 21.0 - 500 °C
Mean
 16.6 µm/m-°C
@Temperature 21.0 - 900 °C
Mean
Thermal Conductivity 23.8 W/m-K
Melting Point 1400 - 1440 °C
Solidus 1400 °C
Liquidus 1440 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.0 - 4.75 %
Carbon, C <= 0.30 %
Copper, Cu <= 0.25 %
Iron, Fe <= 0.60 %
Manganese, Mn <= 0.50 %
Nickel, Ni >= 93 %Including Cobalt
Silicon, Si <= 1.0 %
Sulfur, S <= 0.010 %
Titanium, Ti 0.25 - 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition A
Eagle Brass 301 Austenitic Stainless Steel, 1/2 Hardened
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)

NINCO71 / 17505

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.