Being a hot oil treated version of BT13NPN, BT13SPN is a tube made from a medium weight canvas fabric combined with a phenolic resin that has good physical properties and machining characteristics. Typical applications include textile bobbins, lap spools and structural parts that require good impact strength. |
Cotton, Phenolic, Micarta, EndurX |