MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Avient Bergamid™ A70 UF natur V0 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: PA66 unreinforced general-purpose injection molding grade

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc
@Temperature 23.0 °C
0.0412 lb/in³
@Temperature 73.4 °F
±0.03 g/cm³; DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 70.0 MPa
@Temperature 23.0 °C
10200 psi
@Temperature 73.4 °F
ISO 527-2/50
Elongation at Yield 4.0 %
@Temperature 23.0 °C
4.0 %
@Temperature 73.4 °F
ISO 527-2/50
Tensile Modulus 3.50 GPa
@Temperature 23.0 °C
508 ksi
@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Flammability, UL94 V-0
@Thickness 0.400 - 3.00 mm
V-0
@Thickness 0.0157 - 0.118 in
UL 94
Glow Wire Flammability Index 960 °C
@Thickness 0.400 - 3.00 mm
1760 °F
@Thickness 0.0157 - 0.118 in
IEC 60695-2-12
 
Descriptive Properties
AppearanceOpaque
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
K-Value74.0 to 78.0No Standard; 96% H2SO4
Regional AvailabilityEurope
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6)
Avient Bergadur™ PB40 G15 blue Polybutylene Terephthalate (PBT)
Avient Bergamid™ A70 G25 H U-SO Polyamide 66 (Nylon 66)
Avient Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6)
Overview of materials for Nylon 66/6

PH0POL1390 / 145959

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.