MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
NeXolve Essar™ Stretch 255 Polyimide
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: High temperature colorless elastic polyimide.

NeXolve Essar™ Stretch 255 combines polyimide high temperature survivability and stability with elastomer elasticity and optical clarity into a single polyimide elastomer. Essar™ Stretch 255 is a colorless polyimide elastomer with a wide variety of uses in display applications, space structures, thermal insulation, electrical insulators, industrial tapes and advanced composites. For applications requiring transparency, traditional polyimides are highly absorptive in the UV and blue region, and absorb significant amounts of energy, leading to high thermal loads.

Essar Stretch™ 255 provides high optical clarity in combination with elastomer compliance. Essar™ Stretch 255 is solvent soluble and forms a tough, conformal coating upon cure. Essar™ Stretch 255 is provided as a film in continuous rolls, or as a liquid resin for spray or flow casting operations.

Information Provided by NeXolve Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 19.0 MPa
@Thickness 0.0500 mm
ASTM D882-02
Elongation at Break 80 %
@Thickness 0.0500 mm
ASTM D882-02
Tensile Modulus 0.0410 GPa
@Thickness 0.0500 mm
ASTM D882-02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 220 µm/m-°C
@Thickness 2.00 mm,
Temperature -125 - 20.0 °C
ASTM E831-06
Glass Transition Temp, Tg 33.0 °CDSC; ASTM E1356-03
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
@Wavelength 549 nm
Abbe; ASTM D542-00
UV Transmittance 50 %
@Thickness 0.0500 mm,
Wavelength 392 nm
50% Transmission UV Cutoff
 
Descriptive Properties
ApplicationsAdvanced Composites
 Conformal Encapsulants
 Display Applications
 Electrical Insulators
 Industrial Tapes
 Space Structures
 Thermal Insulation
CharacteristicsForms a tough conformal coating
 High heat stability
 High optical clarity, low visible light absorption
 Highly elastic, greater than 100% recoverable elastic strain
 Low temperature curing
 Solvent soluble
Solar Absorptivity0.12 mil thickness; ASTM E903-96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
Overview of materials for High Density Polyethylene (HDPE), Film Grade
NeXolve Thermalbright® N Polyimide Film
NeXolve Novastrat® 905 Polyimide
NeXolve LaRC™-CP1 Polyimide

PNEXOL903 / 171857

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.