MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Edistir® N 3380 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. N 3380 belongs to the third generation of Edistir® GPPS. Suitable for direct gassing extrusion, biaxial oriented film and sheet, glass clear sheet and panels. Also used in injection molding of medium wall-thickness transparent parts. Thanks to N 3380, injected items will be brighter and neutral colored in line with more sophisticated market needs. The new color will not be noticeable in covered applications.

Applications: Suitable for foamed packaging trays, clear panels for shower cubicles, insulation boards (XPS), OPS for labels and packaging, clear molded fridge components, petri dishes and technical parts.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.650 g/ccISO 60
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cmISO 294/4
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ISO 2039/2
Tensile Strength at Break 49.0 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ISO 527
Tensile Modulus 3350 MPa1 mm/min; ISO 527
Flexural Strength 91.0 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 1.70 kJ/m²
@Thickness 4.00 mm,
Temperature -30.0 °C
ISO 180/1A
 1.90 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 7.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.50e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 50 Hz
IEC 60250
Dielectric Strength 70.0 kV/mmIEC 60243
Dissipation Factor 0.00020
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 425 VSol.A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CASTM D 696
Thermal Conductivity 0.170 W/m-KISO 8302
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C120°C/h, annealed; ASTM D 648
Vicat Softening Point 101 °C
@Load 5.10 kg
50°C/h; ISO 306/B
 106 °C
@Load 1.02 kg
50°C/h; ISO 306/A
Flammability, UL94 HB
@Thickness 1.50 mm
Glow Wire Test 650 °C
@Thickness 1.60 mm
IEC 60695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9879 / 265573

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.