MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ V2000DM PBT (Asia)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccASTM D792
Density 1.32 g/ccISO 1183
Water Absorption 0.34 %23°C/sat; ISO 62
Moisture Absorption 0.0800 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.021 - 0.024 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 34 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 35.4 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPa50 mm/min; ASTM D638
 55.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 59.0 MPa50 mm/min; ISO 527
 59.0 MPa50 mm/min; ASTM D638
Elongation at Break 15 %50 mm/min; ISO 527
 100 %50 mm/min; ASTM D638
Elongation at Yield 7.0 %50 mm/min; ISO 527
 20 %50 mm/min; ASTM D638
Tensile Modulus 2600 MPa1mm/min; ISO 527
 2800 MPa5 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2500 MPa2 mm/min; ISO 178
 2570 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 46.0 J/mASTM D256
Izod Impact, Unnotched NB
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 2.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 4.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 54.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 54.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 185 °CRate B/120; ISO 306
 185 °CRate B/50; ASTM D1525
 186 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 255 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 255 °C
Zone 3 245 - 260 °C
Melt Temperature 245 - 260 °C
Mold Temperature 50.0 - 75.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00130 - 0.00250 cm
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10296 / 243763

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.