MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 30 XTS1 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA 6, 30% glass fibers, injection molding, heat-aging stabilized, notably high heat-aging stability

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/ccISO 60
Density 1.36 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0025 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0063 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %5 mm/min; ISO 527-1,-2
 3.0 %Nominal, 50 mm/min; ISO 527-1,-2
Tensile Modulus 9500 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 250 MPa2 mm/min; ISO 178-A
Flexural Modulus 9400 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 3.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched 9.00 kJ/m²
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 108 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 221 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-1,-2
Shrinkage, MD 0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.14 %
@Treatment Temp. 120 °C,
Time 14400 sec
60x60x2; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °Cinjection molding
 280 - 300 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 120 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 30 XTS1 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 XTS1 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 H2.0 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® AKV 35 XTS1 901510 Nylon 66 (PA66), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 35 HR H2.0 901510 Nylon 66 (PA66), 35% Glass Fiber Reinforced, Conditioned

PLANW9396 / 208223

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.