MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SIL® EL-90 Fumed Silica
Categories: Other Engineering Material

Material Notes: CAB-O-SIL EL-90 fumed silica is a high purity product with a nominal BET surface area of 90 m2/g. The product is designed for use in dispersion and slurry formulations used to polish silicon wafers, a process commonly known as Chemical Mechanical Planarization, CMP.

CAB-O-SIL EL-90 fumed silica is characterized by:

  • High chemical purity
  • Narrow surface area range
  • Narrow particle size distribution
  • High level of product consistency
Chemical Mechanical Planarization is a critical process in the semiconductor manufacturing industry. CMP facilitates smooth, clean, and planar surfaces by using carefully formulated and controlled fumed metal oxide dispersions and other chemicals in conjunction with specially designed equipment and polishing pads. Cabot Corporation was one of the first providers of abrasives for CMP. Throughout the years, Cabot fumed silica has developed a proven track record of high performance and consistency at high volume production. Continuous investment in Cabot’s fumed silica manufacturing technology allowed our products to evolve with the increasingly demanding semiconductor industry and provide reliable and consistent performance in polishing applications. Additionally, Cabot has global presence, with manufacturing and technical support in Asia, North America, and Europe.
CAB-O-SIL EL-90 Fumed Silica Product Performance: The key performance features of CAB-O-SIL EL-90 fumed silica in a model slurry formulation are shown in the figures below. For the purposes of evaluating the abrasive, a model slurry formulation was used for testing. The model formulation consisted of 12% CAB-O-SIL EL-90 fumed silica in 18 M??deionized water at pH 11 (KOH stabilized).

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Surface Area 90 m²/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT077 / 315812

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.