MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wolf Kunststoff INKUPAL 20CV200 B7L
Categories: Polymer; Thermoplastic

Material Notes:

Information provided by Wolf Kunststoff

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
Water Absorption <= 1.0 %RMC 93%; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 206 MPaDIN EN ISO 527
Elongation at Break 2.0 %maximum force; DIN EN ISO 527
Tensile Modulus 14000 MPaDIN EN ISO 527
Flexural Strength 320 MPaDIN EN ISO 178
Flexural Modulus 12000 MPaDIN EN ISO 178
Flexural Strain at Yield 3.4 %DIN EN ISO 178
Charpy Impact Unnotched 39.0 kJ/m²EN ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²EN ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1e+05IEC 60093
Surface Resistance <= 1e+05IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µm/m-°C
@Temperature 100 °C
ISO E 830
Thermal Conductivity 0.900 W/m-KDIN 52612
Maximum Service Temperature, Air 102 °Clong term; UL 746B
 157 °C3 h
Flammability, UL94 V-0
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEDEX3015 / 250072

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.