MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Noveon® AA-1 POLYCARBOPHIL USP
Categories: Polymer; Thermoplastic

Material Notes: Noveon® AA-1 polycarbophil USP meets the limits cited in the current edition of the following monograph:
  • United States Pharmacopeia/National Formulary (USP/NF) monograph for Polycarbophil
  • Class I solvents including benzene and 1,2 dichloroethane (to be avoided) and class II solvents including methylene chloride and cyclohexane (to be limited) per ICH Q3C guidance are NOT used as raw materials or in the production of this excipient.

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH <= 4.01% Dispersion; USP/NF
Brookfield Viscosity 2000 - 12000 cPRVT, 20 rpm, neutralized to pH 7.3 - 7.8, 0.2 wt% mucilage, spindles #4 and #5; Lubrizol 430-I
Ash <= 4.0 %Residue on Ignition; USP/NF
 
Descriptive Properties
Absorbing Power>62 g/gUSP/NF
AppearanceWhite powder
IdentificationPass1:200, Colorimetric test, USP/NF
 Pass1:200, Gel formation test, USP/NF
Loss on Drying<1.5%USP/NF
OdorSlightly acetic
Residual Monomer<3000 ppmFree acrylic acid, Lubrizol SA-005
Residual Solvent<0.45%Ethyl acetate, Lubrizol SA-009

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR8012 / 238960

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.