Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Fungus Resistant; Low Temperature Flexibility Uses: Military Applications; Tubing Agency Ratings: MIL-631-D, Grade A, Class I, Gorm U, Type F; MIL 1-7444-D Grade B, Class I, Category I Form: Pellets Processing Method: Extrusion Information provided by Teknor Apex |