MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC SABIC® LDPE 2402H3W PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE 2402H3W is a high gloss, general purpose grade with a high level of anti block and slip agent. This grade offers good optical properties and a very good draw down ability. Application SABIC® LDPE 2402H3W is typically used for thin high gloss films used for automatic packaging purposes. Due to very low migration levels, SABIC® LDPE 2402H3W can also be used for food applications. Film properties Film properties have been measured at film of 25 µm with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D1505
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 11.0 MPaISO 527-3
Film Elongation at Break, MD >= 200 %ISO 527-3
Film Elongation at Break, TD >= 500 %ISO 527-3
Tensile Modulus 190 MPaMD; ISO 527-3
 200 MPaTD; ISO 527-3
Coefficient of Friction 0.20ASTM D1894
Tear Strength 35.0 kN/mTD; ISO 6383-2
 70.0 kN/mMD; ISO 6383-2
Dart Drop Total Energy 200 J/cmASTM D4272
Film Tensile Strength at Break, MD 28.0 MPaISO 527-3
Film Tensile Strength at Break, TD 20.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 98.0 °Cat 10 N (VST/A); ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %ASTM D1003
Gloss 60 %45°; ASTM D2457
 
Descriptive Properties
Blocking<5 gSABIC method
Re-blocking<5 gSABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10973 / 244440

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.