MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Schott D 263® M Glass for Microscopy Cover Slips
Categories: Ceramic; Glass; Optical

Material Notes: The cover glass type D 263® M is a colorless borosilicate Glass which is produced by a SCHOTT specific down-draw method. It is available in different stock sheet sizes with thicknesses ranging from 0.1 mm to 0.21 mm. D 263® M is a perfect choice as cover glass for microscopic analysis and meets the requirements specified in ISO 8255-1 and DIN ISO 8255-1. The chemical composition of D 263® M ensures valid and reliable research results due to its low auto fluorescence and high chemical resistance.

Application: Cover glass in microscopy for medical, biological and research work

  • High luminous transmittance
  • Colorless appearance
  • Excellent cosmetic quality
  • Easy to cut using the scribe and break method
  • Excellent flatness
  • Resistant to chemical attack
  • Refractive index finely adapted to microscopes
  • Low auto-fluorescence
  • Easy to separate in automatic cover slippers due to protective coating
  • Tight thickness control
  • Resistance to environmental conditions ensure high durability
  • Good cell growth
  • Thickness for high-performance applications available

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.51 g/ccAnnealed at 40°C/h
Thickness 0.145 microns
 0.175 microns
 0.210 microns
 100 microns
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.7
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.20 µm/m-°C
@Temperature 20.0 - 300 °C
Transformation Temperature, Tg 557 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.523
@Wavelength 589.3 nm
D
 1.525
@Wavelength 546.1 nm
e
Transmission, Visible 91.7 %D65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott D 263 Thin Borosilicate Glass
Corning Pyrex® 7740 Borosilicate Glass Sheet
Borosilicate Glass, Low Expansion
Borosilicate Glass
Schott D 263® T eco Thin Borosilicate Optical Glass

CSGT9943 / 183196

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.