Borcell HE1105 is a high-density polyethylene (HDPE) compound formulated with specific viscosity and melt strength characteristics. Borcell HE1105 is intended for the insulations of coaxial cables using gas foaming processes and is suitable for constructions exceeding 10-mm diameter over the dielectric. Information provided by the Manufacturer. |