MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Plexus® MA2030 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Plexus® MA2030 is a two-part methacrylate adhesive designed for structural bonding of composite, thermoplastic, and metal assemblies. MA2030 was uniquely formulated to eliminate problems associated with adhesive sag and slide, even when applied to a vertical surface. In addition, MA2030 does not boil in gaps up to 1.5 inches thick. Combined at a 10:1 ratio at 75°F (24°C), it has a working time of approximately 35 minutes and achieves 500 psi and 1000 psi in approximately 70 and 90 minutes, respectively. As with most other Plexus methacrylate systems, MA2030 requires little to no surface preparation. MA2030 provides a unique combination of excellent fatigue endurance, outstanding impact resistance, and superior toughness. MA2030 is supplied ready to use to be dispensed as a non-sagging gel.

Excellentl resistance to: ? Hydrocarbons ? Acids and Bases (pH 3-10) ? Salt Solutions Susceptible to: ? Polar Solvents ?Strong Acids and Bases. Recommended for: ? ABS ? Acrylics ? FRP ? Gel coats ? PVC ? Polyesters (including DCPD modified) ? Select metals? Styrenics? Urethanes (general)? Vinyl Esters ( Exterior applications require the use of coatings or primers that inhibit oxidation of the steel.)

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.86 lb/galadhesive. Uncured.
 7.95 lb/galCured
 8.90 lb/galActivator. Uncured.
Volatile Organic Compounds (VOC) Content <= 10 g/lDuring cure
Viscosity 180000 - 220000 cP
@Temperature 22.2 °C
Adhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3000 - 3400 psiASTM D638
Elongation at Break 90 - 125 %ASTM D638
Tensile Modulus 90000 - 120000 psiASTM D638
Adhesive Bond Strength 1600 - 2100 psiLap Shear Cohesive Strength; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point 51.0 °F
 
Processing PropertiesOriginal ValueComments
Working Life 25.0 - 35.0 min
@Temperature 23.3 °C
Shelf Life 10.0 MonthCartridges
 10.0 MonthActivator (B side)
 13.0 MonthAdhesive (A side)
 
Descriptive Properties
Fixture Time (mins)70 to 9074°F cure. Varies with bond gap and temperature.
Gap Filling (in)0.03 to 1.5Room temperature cure.
Mix Ratio by volume10 to 1Adhesive to Activator. Room temperature
Mix Ratio by weight8.83 to 1.0Adhesive to Activator. Room temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9008 / 239518

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.