MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Sealants & Adhesives Concrete Silicone 2 100% waterproof sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Concrete Silicone 2 sealant is 100% waterproof and ideal for vertical and horizontal applications on concrete, mortar and stone projects. This sealant has a fast cure and can be exposed to rain or water in as little as 30 minutes. Concrete Silicone 2 sealant is weatherproof, permanently flexible, shrink-proof and crack-proof, and offers strong adhesion. It can be applied to either wet or dry surfaces. This high performance and durable sealant is both sun-proof and freeze-proof and will not breakdown or wash away when exposed to harsh weather. Backed by a lifetime guarantee.

Features: Fast cure: 30-minute tack free and 24-hour full cure. 30-minutes rain and water exposure. 100% weatherproof, freeze-proof and sun-proof, will not degrade in harsh climates. Meets ASTM C-920 Class 25 specifications. Permanently flexible to keep gaps sealed. Shrink-proof and crack-proof. Will never break down due to extreme weather conditions. Resist mold with 10-year mold-free product protection. Excellent adhesion for wet or dry applications. Freeze/thaw stability. Non-paintable.

Applications: Concrete Silicone 2 sealant is used for both vertical and horizontal use with concrete, mortar, brick and stone in a wide variety of applications including sidewalks, driveways, porches, cinder block foundations, asphalt, around wire/pipes and tuck/repairing masonry applications.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccCured.
Volatile Organic Compounds (VOC) Content <= 28 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 15ASTM D2240
Tensile Strength 1.00 MPaASTM D412
Elongation at Break 347 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull Cure
Tack-Free Time 30.0 min50% RH; ASTM C679
Working Life 5.00 - 10.0 min
 
Descriptive Properties
AppearancePaste
Carb Chem Curing VOC< 3.0 wt%
ColorLight GrayGESIL2CONCRETE
Consistency / Sag< 0.2 inchesASTM D2202
Joint Movement Capability±25%ASTM C719.
OdorLight Ammonia
Rain Ready30 minutes
UV & Weathering ResistanceExcellent30 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9959 / 265774

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.