Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:- They have low density.
- They are highly resistant to chemicals and solvents.
- They are easy to process and color and are easy to overmold.
- They can be decorated easily by means of heat transfer printing.
- They have excellent impact strength at low temperatures.
- Their hardness and flexibility can be varied over a wide range.
- They have high elasticity and good recovery.
- Their mechanical properties are only slightly temperature-dependent.
- They are free of volatile or migrating plasticizers.
Applications: decorative and protective films for sports articles and interior/exterior designs on automobiles Information provided by degussa. Evonik Industries is the successor company to Degussa. |