MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Silberline Sparkle Silver Ultra™ 6756
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Sparkle Silver Ultra™ grades are very bright lenticular automotive aluminum pigments. They offer a very smooth patina and narrow particle size distribution, allowing the formulator to create very smooth, brilliant masstones or clean vibrant colors. SSUs are designed for the stylist to raise the bar in terms of metallic effects and creativity.

Applications: Automotive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/cc
Bulk Factor 0.073
Volatiles 28 %
Particle Size 12 µm
Particle Mesh Size <= 325 Mesh0.01% retained
 
Descriptive Properties
SolventsMineral Spirits/High Flash

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Malvern Minerals Wollastokup® FF Silane Treated Wollastonite
Malvern Minerals Novacite® Daper Untreated Lamellar Quartz Filler/Extender
Imerys ULTRAFIBRE® II Wollastonite
Imerys NYGLOS® 2 Wollastonite
Imerys NYAD® G Special Wollastonite

ESIBER046 / 5801

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.