NORYL GTX™ 600 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance, and excellent chemical resistance. NORYL GTX600 resin may be an excellent candidate for exterior automotive applications such as wheel covers. Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Low Warpage Information provided by SABIC |