MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco ISO 460 Synthetic Wheel Motor Lubricant EP
Categories: Fluid; Lubricant

Material Notes: Features
  • Chevron Synthetic Wheel Motor Lubricants EP are superior quality industrial EP gear lubricants. Their advanced formulation provides superior load carrying and antiwear properties; protection against rust, corrosion, foaming, and oxidation; and excellent demulsibility. This results in outstanding performance in most types of industrial gearboxes, exemplified by the FZG pass stage result of >12.
  • These products possess very high shear stability even under heavily loaded, high speed conditions in industrial gears.
  • The low pour point and very good low temperature fluidity of Chevron Synthetic Wheel Motor Lubricants EP impart improved lubrication during startup at low temperatures. The superior viscosity-temperature characteristics also provide a much higher oil viscosity at operating temperature compared to a mineral oil product of the same ISO grade. This results in increased oil film thickness and better antiwear protection for both bearings and gears.
  • A unique property of the synthetic base oil is a low traction coefficient, resulting in improved gear efficiency, energy savings, less friction, less wear, and lower operating temperatures compared to conventional mineral oil products.
  • Drain intervals can be extended longer than conventional mineral oil products. That means fewer oil changes, reduced maintenance costs, and less used oil disposal.

Applications

Chevron Synthetic Wheel Motor Lubricants EP are especially recommended for off-highway electric wheel motors used in mining haul trucks. The products are approved by General Electric for use in their wheel motors, which can be found on mining trucks made by Komatsu, Haul Pack, Terex, Hitachi, and Liebherr.

In addition to wheel motors, Chevron Synthetic Wheel Motor Lubricants EP are suitable for all types of enclosed industrial gearboxes. They are especially recommended for gearboxes running continuously at temperatures up to 107°C (225°F) or exposed to very cold temperatures, or under severe service conditions, such as heavy loads or low speeds. These products also provide excellent protection for bearings operating under similar conditions.

Chevron Synthetic Wheel Motor Lubricants EP meet the requirements of:

  • U.S. Steel 224
  • AGMA 9005 EP
  • General Electric Transportation Systems D50E27
  • General Atomics-Power Inverters Division

Key Words: CPS Number: 226816; MSDS Number: 11331
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29 °
Viscosity Measurement 124Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 2427 SUS
Saybolt Viscosity at 210°F 182 SUS
Kinematic Viscosity at 40°C (104°F) 460 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 37.5 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Timken Test 70.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 225 °F
Pour Point -32.0 °CASTM D97
Flash Point 238 °CASTM D92
 
Descriptive Properties
FZG Gear Wear Test, Failure Load Stage12
Rust Prevention, ASTM D665Pass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive, Flexible
ChevronTexaco ISO 680 Synthetic Wheel Motor Lubricant EP
AISI Type W2 Tool Steel, water quenched at 775°C (1425°F), and tempered
AISI Type W2 Tool Steel, water quenched 775°C (1425°F), tempered 700°C (1300°F)
AISI Type O2 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 260°C

WCHEV222 / 74837

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.