MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
KaMin Polyfil® 35 Kaolin Clay - Waterwashed
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Coarse kaolin, with the lowest oil absorption, for extending without reinforcement, milled powder form.

Industry: Rubber & Plastic

Uses: Non-Black Rubber, General Rubber Goods, General Plastics, SMC/BMC, Mold Release

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Bulk Density 28.0 - 31.0 lb/ft³Loose
Brightness 84 %Reflectance (TAPPI)
Oil Absorption 27 %
Fineness >= 4Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %As Produced
Particle Size 4.0 µmAverage Stokes Equivalent Diameter
 7.0 µmMedian (Malvern Laser)
Particle Mesh Size 325 Mesh0.03% Retained
pH 7100 g/250 ml H2O Slurry
Specific Surface Area 9.4 m²/gBET
 
Descriptive Properties
Bulking Value21.7 lb.gal
CAS Number1332-58-7
Crystalline Silica (quartz)<0.1%
Physical FormDry
Shipping PointMacon, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite SUMILITE® ELC-4970GS Glass Epoxy Laminate
Omya OMYACARB® 5 - FL Calcium Carbonate
Hexcel® HexPly® F522 Epoxy Resin, 120 Glass Fabric

CKAMAN936 / 178407

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.