MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Vac-Pak® HS8171PS Adhesive tape
Categories: Polymer; Adhesive; Tape

Material Notes: Description: Adhesive tape. Ideally suited to masking applications.

Features & Benefits:

  • High temperature nylon tape with a pressure sensitive, rubber-base adhesive on one side.
  • Designed to strip cleanly from the part during masking operations in high temperature/pressure applications.
  • High elongation properties provide a high degree of conformability.
  • Rubber based adhesive allows for use on parts where subsequent painting or bonding is necessary.
  • High stretch and thinness offer excellent conformability and clean, sharp edges.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 38.0 micronsAdhesive
 50.0 micronsTape
 88.0 micronsTotal
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 500 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCYTED239 / 180541

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.