MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound MD000ISC Polypropylene, Unspecified (PP, Unspecified)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP STAT-KON MD000ISC compound is based on Polypropylene (PP) resin containing conductive carbon powder. Added features of this grade include: Electrically Conductive, High Impact, Heat Stabilized.

Features: High Impact Resistance,Heat Stabilized,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccISO 1183
 0.980 g/ccASTM D792
Moisture Absorption 0.0300 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm24hrs; ASTM D955
 0.016 - 0.018 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm24hrs; ASTM D955
 0.016 - 0.018 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17.0 MPaASTM D638
 17.0 MPaISO 527
Tensile Strength, Yield 18.0 MPaISO 527
 21.0 MPaASTM D638
Elongation at Break 133.8 %ASTM D638
Elongation at Yield 9.0 %ASTM D638
Tensile Modulus 480 MPa50 mm/min; ASTM D638
 1100 MPa1 mm/min; ISO 527
Flexural Strength 27.0 MPaASTM D790
 27.0 MPaISO 178
Flexural Modulus 1130 MPaASTM D790
 1200 MPaISO 178
Izod Impact Notched 833 JASTM D256
Izod Impact, Unnotched 1553 J/mASTM D4812
Izod Impact, Notched (ISO) 65.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 112 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 24.0 Jpeak; ASTM D3763
Impact Test 31.0 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 10 - 1.00e+6 ohmASTM D257
Static Decay <= 0.010 sec5000V to <50V; FTMS101B
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 101 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 101 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 119 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 119 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 52.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 215 - 225 °C
Zone 3 240 - 250 °C
Melt Temperature 225 - 250 °CInjection Molding
Mold Temperature 30.0 - 50.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81317 / 289264

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.