MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for Unalloyed/Modified Titanium
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Unalloyed/Modified Titanium". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.50 - 4.81 g/ccAverage value: 4.52 g/cc Grade Count:42
 
Chemical PropertiesOriginal ValueComments
Thermal Neutron Cross Section 5.60 barns/atomAverage value: 5.60 barns/atom Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 90.0 - 265Average value: 180 Grade Count:21
Hardness, Knoop 99.0 - 296Average value: 200 Grade Count:11
Hardness, Rockwell B 23.0 - 104Average value: 83.9 Grade Count:15
Hardness, Rockwell C 11.0 - 32.0Average value: 19.1 Grade Count:8
Hardness, Vickers 100 - 280Average value: 196 Grade Count:10
Tensile Strength, Ultimate 240 - 1170 MPaAverage value: 487 MPa Grade Count:37
Tensile Strength, Yield 170 - 1100 MPaAverage value: 395 MPa Grade Count:37
Elongation at Break 8.00 - 37.0 %Average value: 24.0 % Grade Count:37
Reduction of Area 15.0 - 70.0 %Average value: 36.3 % Grade Count:16
Modulus of Elasticity 100 - 120 GPaAverage value: 106 GPa Grade Count:20
Compressive Yield Strength 340 - 550 MPaAverage value: 404 MPa Grade Count:5
Compressive Modulus 107 - 114 GPaAverage value: 110 GPa Grade Count:11
Notched Tensile Strength 620 - 900 MPaAverage value: 750 MPa Grade Count:5
Ultimate Bearing Strength 680 - 1000 MPaAverage value: 882 MPa Grade Count:5
Bearing Yield Strength 565 - 900 MPaAverage value: 688 MPa Grade Count:5
Poissons Ratio 0.210 - 0.370Average value: 0.339 Grade Count:15
Fatigue Strength 116 - 517 MPaAverage value: 272 MPa Grade Count:15
Fracture Toughness 66.0 - 140 MPa-m½Average value: 88.2 MPa-m½ Grade Count:3
Shear Modulus 36.0 - 45.0 GPaAverage value: 40.6 GPa Grade Count:15
Shear Strength 380 - 450 MPaAverage value: 398 MPa Grade Count:4
Charpy Impact 15.0 - 310 JAverage value: 95.7 J Grade Count:7
Coefficient of Friction 0.680 - 0.800Average value: 0.740 Grade Count:4
Bend Radius, Minimum 2.00 - 5.00 tAverage value: 2.86 t Grade Count:12
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000420 - 0.0000600 ohm-cmAverage value: 0.0000525 ohm-cm Grade Count:19
Magnetic Permeability 1.00Average value: 1.00 Grade Count:4
Magnetic Susceptibility 3.98e-8 - 0.00000317Average value: 0.00000108 Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.41 - 19.9 µm/m-°CAverage value: 10.6 µm/m-°C Grade Count:20
Specific Heat Capacity 0.520 - 0.555 J/g-°CAverage value: 0.530 J/g-°C Grade Count:16
Thermal Conductivity 15.9 - 22.0 W/m-KAverage value: 17.9 W/m-K Grade Count:20
Melting Point 1660 - 1670 °CAverage value: 1660 °C Grade Count:14
Liquidus 1660 - 1670 °CAverage value: 1660 °C Grade Count:14
Maximum Service Temperature, Air 316 - 540 °CAverage value: 474 °C Grade Count:10
Beta Transus 882 - 960 °CAverage value: 912 °C Grade Count:21
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) 0.560Average value: 0.560 Grade Count:14
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.0800 - 0.100 %Average value: 0.0945 % Grade Count:40
Hydrogen, H 0.00500 - 0.0150 %Average value: 0.0143 % Grade Count:40
Iron, Fe 0.150 - 0.600 %Average value: 0.308 % Grade Count:40
Molybdenum, Mo 0.200 - 0.400 %Average value: 0.300 % Grade Count:5
Nickel, Ni 0.600 - 0.900 %Average value: 0.770 % Grade Count:5
Nitrogen, N 0.0300 - 0.0500 %Average value: 0.0370 % Grade Count:40
Oxygen, O 0.120 - 0.400 %Average value: 0.270 % Grade Count:40
Palladium, Pd 0.0500 - 0.250 %Average value: 0.149 % Grade Count:14
Titanium, Ti 97.7 - 100 %Average value: 99.1 % Grade Count:43

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Alpha/Beta Titanium Alloy
Overview of materials for Beta Titanium Alloy
Overview of materials for Stainless Steel
Titanium, Ti
Overview of materials for Alpha/Near Alpha Titanium Alloy

M01073 / 81701

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.