MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
United Cast Bar Unibar 300 Continuously Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Unibar 300 is alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and an excellent surface finish. Noise and vibration damping are excellent in this grade.

Unibar 300 can be hardened by conventional methods, to Rc 50 on the bar surface.

Information provided by United Cast Bar Ltd.

Key Words: EN-1561-GJL-300 GG30; Meehanite GB300.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 190 - 260
@Load 3000 kg
10 mm ball
Tensile Strength 195 MPa
@Diameter 150 - 300 mm
 210 MPa
@Diameter 80.0 - 150 mm
 240 MPa
@Diameter 40.0 - 80.0 mm
 270 MPa
@Diameter 20.0 - 40.0 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.95 - 3.45 %
Iron, Fe 92.63 - 94.26 %as balance
Manganese, Mn 0.55 - 0.75 %
Phosphorus, P 0.10 - 0.20 %
Silicon, Si 2.1 - 2.9 %
Sulfur, S 0.040 - 0.070 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
United Cast Bar Unibar 250 Continuously Cast Iron
United Cast Bar Unibar 200 Continuously Cast Iron
Gray Cast Iron, ASTM A 48 Class 40
ASTM class 30 Standard gray iron test bars, as cast
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron

NUNITED03 / 160450

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.