MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 20 FN20 DUS013 000000 Nylon 6, 20% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: PA 6, 20% glass fibers, injection molding, halogen-free flame retardant

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0060 cm/cm60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0070 cm/cm60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPad.a.m.; ISO 527-1, -2; 5 mm/min
Elongation at Break 3.0 %d.a.m.; ISO 527-1, -2; 5 mm/min
Tensile Modulus 6100 MPad.a.m.; ISO 527-1, -2; 1 mm/min
Flexural Strength 150 MPa
@Strain 5.0 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Yield Strength 135 MPa
@Strain 3.5 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Modulus 5700 MPad.a.m., 2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²d.a.m.; ISO 180-1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²d.a.m.; ISO 180-1U
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 500 Vd.a.m.; Solution A; UL 746A
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C10°C/min; ISO 11357-1, -3
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75-1, -2
Vicat Softening Point 205 °C
@Load 5.10 kg
120°C/hour; ISO 306
Flammability, UL94 V-2
@Thickness 1.50 mm
 V-2
@Thickness 0.750 mm
 V-2
@Thickness 3.00 mm
Glow Wire Flammability Index 960 °C
@Diameter 0.800 mm
IEC 60695-2-12
 960 °C
@Diameter 1.50 mm
IEC 60695-2-12
 960 °C
@Diameter 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
 260 °Cfor test specimens; ISO 294
Mold Temperature 80.0 °Cfor test specimens; ISO 294
 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2 - 6 hour
Moisture Content 0.030 - 0.070 %residual; Karl Fischer Test
 
Descriptive Properties
ISO Short NameISO 1874-PA 6, GFHR, 12-060, GF20; ISO 1043-PA GF FR(30)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber
Celanese Rynite® FR530 NC010 PET-GF30FR(17)
Celanese Rynite® FR530 BK507 PET-GF30FR(17)
Envalior Durethan® BKV 25 FN27 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 25 FN01 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry

PLANX0625 / 133588

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.