MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Paxon™ AL55-003 Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: AL55-003 is a blow molding grade high density polyethylene offering a good combination of stiffness and stress crack resistance.

Availability: Latin America, North America and South America

Additive:

  • Thermal Stabilizer: Yes
  • Antistatic: No
Applications:
  • Drainage Pipes
  • Food packaging
  • Household and Industrial chemical containers
  • Pharmaceutical Packaging
  • Thermoformed Parts
  • Thin Gauge Sheet
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D4883
ESCR 100% Igepal® 30 hourASTM D1693 Condition B
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4100 psiASTM D638
Elongation at Break 560 %ASTM D638
Flexural Modulus 190000 psiMethod1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 90.0 ft-lb/in²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 260 °FASTM D1525
Brittleness Temperature <= -105 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5440 High Density Polyethylene
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
ExxonMobil Paxon™ AM55-003 Blow Molding Resin
ExxonMobil Paxon™ AG45-004 Blow Molding Resin

PEXB098 / 37403

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.