MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® PBT 700/1 GF30 PTFE15 PBT, 30% Glass/15% PTFE Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled

Material Notes: Base Polymer: Polybutylene Terephthalate

Filler/Additive System: 30% Glass fibers, 15% PTFE

Special Features: Improved sliding/wear, high stiffness

Market Segment: Automotive, Machinery

Application Area: Gear wheels, roller bearings

Typical Applications: Functional components, bearings and sliding elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 125 MPaISO 527
Elongation at Break 2.8 %ISO 527
Tensile Modulus 10400 MPaISO 527
Flexural Strength 200 MPaISO 178
Flexural Modulus 9300 MPaISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 70.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.50 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
Vicat Softening Point 214 °CB50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °CInjection molding
Mold Temperature 80.0 - 120 °CInjection molding
Drying Temperature 100 - 120 °C
@Time 14400 - 28800 sec
in air circulating dryer
 100 - 120 °C
@Time 7200 - 14400 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolybutylene Terephthalate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 2300 G6 HR BK15116 30% Glass Filled PBT
Mocom (ALBIS) ALCOM® PBT 700/1 GF20 PTFE15 PBT, 20% Glass/15% PTFE Reinforced
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer
Ravago Manufacturing Americas Echo® RPPC 30/2 BK Recycled Polypropylene
BASF Ultradur® B 2550 PBT

PALBIS8115 / 242174

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.