MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Redwood Plastics Redco™ TITANIUM UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Redco™ Titanium is specially formulated to be the slickest, strongest and toughest with superior abrasion resistance and the lowest thermal expansion. Developed for the most demanding applications involving impact and sliding, Redco™ Titanium will withstand the most severe environments.

Standard Color: Grey

Typical Applications: Bin liners, hopper liners, flume liners, belt scrapers, skirt boards, chutes, conveyors, silos, cyclones, spoon liners, bunkers, wear strips, feeder liners, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 67ASTM D 785
Tensile Strength <= 36.0 MPaASTM D 638
Tensile Strength, Yield 19.0 MPaASTM D 638
Elongation at Break 400 %ASTM D 638
Flexural Modulus 622 MPaASTM D 790
Izod Impact, Notched (ISO) 78.0 kJ/m²DOUBLE NOTCHED; ASTM D 256A
 NBASTM D 256A
Coefficient of Friction, Dynamic 0.10Against Cr-Plated Steel; ASTM D 1894
Coefficient of Friction, Static 0.12Against Cr-Plated Steel; ASTM D 1894
Abrasion 7.5Sand Slurry, Index (Relative To Steel At 100)
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D 257
Surface Resistance >= 1.00e+16 ohmASTM D 257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°CASTM D 696
Maximum Service Temperature, Air 82.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW004 / 296570

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.