MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
305 Stainless Steel, High tensile bar, wire
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Same corrosion resistance and Type 302, but much lower rate of work hardening. Excellent cold formability, good free spinning and cold heading properties, recommended for severe cold drawing. Applications include electronic parts and other drawn applications.

Key Words: UNS S30500,, DIN 1.4303, UNI X8 CrNi 19 10, JIS SUS 305, SUS 305 J1, ISO 4954 X5CrNi1812E, ISO 683/13 13, 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1690 MPa
Elongation at Break 25 %
@Diameter <=3.96 mm
Reduction of Area 40 %
@Diameter <=3.96 mm
Modulus of Elasticity 193 GPa
Shear Modulus 86.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.008at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1455 °C
Solidus 1400 °C
Liquidus 1455 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.12 %
Chromium, Cr 18 %
Iron, Fe 67 %
Manganese, Mn <= 2.0 %
Nickel, Ni 12 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed
303 Stainless Steel, annealed bar
305 Stainless Steel, annealed, wire
304 Stainless Steel
Wingate Alloys Winco TGP Turned, Ground and Polished Heat-Treated High Tensile Alloy Steel

MQ305N / 171829

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.