MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM 2 Component System  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Molding Process.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 - 0.950 g/cc
@Temperature 25.0 °C
HY2954 cycloaliphatic amine hardener; ISO 1675
 1.10 - 1.20 g/cc
@Temperature 25.0 °C
RTM 120 bisphenol epoxy resin containing reactive diluent; ISO 1675
Viscosity 70 - 120 cPHY2954 cycloaliphatic amine hardener; DIN 53015
 100 - 140 cPRTM 120 bisphenol epoxy resin containing reactive diluent; DIN 53015
 >= 100 cP
@Temperature 60.0 °C
Initial Mix Viscosity (Hoeppler)
 200 cP
@Temperature 40.0 °C
Initial Mix Viscosity (Hoeppler)
 500 - 700 cP
@Temperature 25.0 °C
Initial Mix Viscosity (Hoeppler)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 71.0 - 77.0 MPaCure: 1h/80°C/140°C; ISO R 527-1966
 822 MPaTensile Warp, Dry/RT; Pr EN 2561
 829 MPa
@Temperature 80.0 °C
Tensile Warp, Wet; Pr EN 2561
Elongation at Break 4.5 - 5.5 %ISO R 527-1966
Tensile Modulus 66.0 GPaTensile Warp, Dry/RT; Pr EN 2561
 57.0 GPa
@Temperature 80.0 °C
Tensile Warp, Wet; Pr EN 2561
Compressive Yield Strength 648 MPaCompression Warp, Dry/RT; Pr EN 2850
 689 MPaCompression Weft, Dry/RT; Pr EN 2850
 401 MPa
@Temperature 80.0 °C
Compression Warp, Wet; Pr EN 2850
 475 MPa
@Temperature 80.0 °C
Compression Weft, Wet; Pr EN 2850
Compressive Modulus 61.0 GPaCompression Warp, Dry/RT; Pr EN 2850
Fracture Toughness 0.700 MPa-m½PM 258-0/90
Shear Strength 68.0 MPaI.L.S. Warp, Dry/RT; Pr EN 2563
 51.0 MPa
@Temperature 80.0 °C
I.L.S. Warp, Wet; Pr EN 2563
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 80.0 - 87.0 °FCure: 4h/80°C; Post cure: None
 123 - 130 °FCure: 1 h/80°C; Post cure: 4 h/120°C
 135 - 142 °FCure: 20 min./120°C; Post cure: 4 h/145°C
 136 - 143 °FCure: 1 h/80°C; Post cure: 4 h/160°C
Flash Point >= 175 °CHY2954 cycloaliphatic amine hardener
 >= 185 °CRTM 120 bisphenol epoxy resin containing reactive diluent
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 2.0RTM 120 bisphenol epoxy resin containing reactive diluent
 <= 3.0HY2954 cycloaliphatic amine hardener
 
Processing PropertiesOriginal ValueComments
Gel Time 3.00 - 4.00 min
@Temperature 140 °C
 7.00 - 9.00 min
@Temperature 120 °C
 10.0 - 12.0 min
@Temperature 110 °C
 16.0 - 18.0 min
@Temperature 100 °C
 35.0 - 45.0 min
@Temperature 80.0 °C
 90.0 - 120 min
@Temperature 60.0 °C
 
Descriptive Properties
ColorClear liquidHY2954 cycloaliphatic amine hardener; As-supplied form
 Clear, Pale yellow liquidRTM 120 bisphenol epoxy resin containing reactive diluent; As-supplied form
Epoxy Content (Eq/kg)5.7-6ISO 3001

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Raschig Group 3581 Epoxy
NRI Syntho-Poxy™ HC Epoxy Compound Filler
Mitsubishi Chemical Advanced Materials Duratron™ U1000 PEI Extruded Unfilled Polyetherimide
Lord Adhesives Circalok™ 6037 Epoxy Adhesive

PHEXC481 / 99300

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.