SABIC® PPcompound 7693 is a very high flow mineral filled modified polypropylene. Material properties include very high flow, high stiffness and a good impact resistance. Typical applications include automotive exterior parts such as bumpers, bumper strips and exterior trim. It can be used in painted and unpainted applications with UV stabilization added on demand.
SABIC® PPcompound 7693 is a designated automotive grade.
IMDS ID: 70133104Information provided by SABIC |