MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
American Pignut Hickory Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Carya glabra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.660 g/ccOven Dry Weight/Unseasoned Volume
 64.0 lb/ft³Unseasoned*
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 11.7 ksiStatic Bending*
Flexural Yield Strength 6200 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 1650 ksiStatic Bending*
Compressive Strength 1140 psiPerpendicular to Grain*
 3950 psiParallel to Grain*
 4810 psiMax Crushing Strength Parallel to Grain*
Shear Strength 1370 psiParallel to Grain*
Impact 8.8in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 16900psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 1.34 in-lb/in³Static Bending*
Work to Maximum Load 31.7 in-lb/in³Static Bending*
 
Thermal PropertiesOriginal ValueComments
Shrinkage 7.2 %Tangential; Unseasoned to Oven Dry*
 7.2 %Radial, from green to oven dry
 11.5 %Tangential, from green to oven dry
 17.9 %Volumetric, from green to oven dry
 18.2 %Radial; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4C 12K Standard Modulus Carbon Fiber (12,000 Filaments)
American Pecan Hickory Wood
Hexcel® HexTow® AS4C 6K Standard Modulus Carbon Fiber (6000 Filaments)
Silver Maple (Water Maple, White Maple), Soft Wood
European Field Elm Wood

PTSA050 / 71243

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.