MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ GRM2600L ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0045 - 0.0065 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 2.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 41.0 MPa5 mm/min; ASTM D638
Elongation at Break 55 %5 mm/min; ASTM D638
Tensile Modulus 2410 MPa5 mm/min; ASTM D638
Flexural Yield Strength 75.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 400 J/mASTM D256
Dart Drop, Total Energy 46.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 113 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 230 - 275 °CInjection Molding
Zone 1 170 - 200 °CSheet Extrusion
 195 - 210 °C
Zone 2 180 - 220 °CSheet Extrusion
 210 - 225 °C
Zone 3 190 - 225 °CSheet Extrusion
 230 - 255 °C
Zone 4 200 - 240 °CSheet Extrusion
Adapter Temperature 205 - 250 °CSheet Extrusion
Die Temperature 205 - 250 °CSheet Extrusion
Melt Temperature 215 - 260 °C
 230 - 275 °C
Mold Temperature 50.0 - 80.0 °C
Roll Temperature 90.0 - 95.0 °CRoll Stack Temp - Top
 95.0 - 105 °CRoll Stack Temp - Middle
 100 - 105 °CRoll Stack Temp - Bottom
Drying Temperature 80.0 - 95.0 °CSheet Extrusion
 90.0 - 95.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 4.00 hourSheet Extrusion
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10042 / 243509

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.