MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Perkadox 20S Dibenzoyl peroxide
Categories: Other Engineering Material

Material Notes: Perkadox 20S is a special low-concentration BPO formulation (20% peroxide) for curing mine bolts and chemical anchors. The low concentration allows for transportation as non-ADR grade. The formulation ensures easy mixing and handling.

CAS number: 94-36-0

EINECS/ELINCS No.: 202-327-6

Applications: For some special applications it is desirable to use a dry benzoyl peroxide powder as a catalyst. For these cases the benzoyl peroxide formulation Perkadox 20S was introduced, which is a mixture of benzoyl peroxide and filler. Perkadox 20S can be handled very easily and without risk. It contains no plasticizer and is lower concentrated than the usual benzoyl peroxide formulations, which makes dosing easier. One of the most important applications for Perkadox 20S is as a catalyst for putties based on unsaturated polyester resins. A putty containing an accelerated polyester resin and Perkadox 20S cures rapidly so that after a short time the surface can be sanded and polished.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.588 g/cc
Density 2.29 g/cc
Storage Temperature <= 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 70.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceWhite powder
Assay20.0-21.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY763 / 286286

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.