Properties: Chlorinated Polyethylene CPE-700 is a type for magnetic products. Chlorinated Polyethylene CPE-700 is featured with high magnetic powder addition level, good processibility and low temperature flexibility.Information provided by Shanghai Potomer International Trade Co., Ltd |