MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Aminoethylethanolamine (AEEA) 2-(2-aminoethylamino)ethanol
Categories: Other Engineering Material

Material Notes: Aminoethylethanolamine (AEEA) is a linear molecule with primary and secondary amine groups. AEEA is a colorless liquid, with slightly higher viscosity than EDA and DETA. It is used as an intermediate in the fabrication of detergents, fabric softeners, chelates, fuel additives and coatings.

CAS number: 111-41-1

EINECS/ELINCS No.: 203-867-5

Molecular formula: C4H12N2O

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.024 g/cc
 1.026 g/ccRelative
pH 1225% solution
Viscosity 141 cPDynamic
Molecular Weight 104.15 g/mol
Vapor Pressure 0.0000120 bar
 
Thermal PropertiesOriginal ValueComments
Melting Point -38.0 °C
@Pressure 0.1013 MPa
Boiling Point 243 °C
@Pressure 0.1013 MPa
Flash Point 132 °C
@Pressure 0.1013 MPa
Ignition Temperature >= 150 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.20 %MOA 305
 
Descriptive Properties
AppearanceClear liquid
Assay=99.6%MOA 553
Color= 20 HazenMOA 201
 Colorless
Content=100 ppmEthylene diamine (MOA 558)
OdorAmmonical
Partition coefficient-1.46N-octanol/water, 25°C, log Pow
Vapor Density3.6air = 1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY120 / 285643

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.