EVATANE® 24-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 24-03 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 24-03 brings softness, flexibility and polarity. EVATANE® 24-03 delivers high cohesive strength with any kind of fillers (masterbatchs, HFFR compounds). EVATANE® 24-03 is also very well adapted for the production of cast or blown films. It can also be used as an additive for bitumen.Information provided by Arkema Group |