MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carbon-Core Transom Ceramic Pourable Compound
Categories: Other Engineering Material

Material Notes: Description: CARBON-CORE formulates its Ceramic Pourable Compound with premium polyester resins and high strength ceramic spheres resulting in high tensile and flexural strength. This lightweight compound is ideal for filling large volumes where strength and rigidity are major concerns. The CarbonCore Ceramic Pourable Compound mixes and pours easily from the 5-gallon pail.
  • Excellent rigidity and strength.
  • ?Formulated with premium resins
  • ?Low shrinkage and exotherm
  • ?Low styrene content
  • ?Structural applications where high compressive strength is required
  • ?7 times better Compression strength than plywood

    Information provided by Carbon-Core

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 25000 - 38000 cP20 rpm
Brookfield Viscosity 85000 - 105000 cPRVT, 2.5 rpm, #7 spindle
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1597 psi
Elongation at Yield 9.14 %ASTM 638-82
 
Processing PropertiesOriginal ValueComments
Working Life 38.0 - 52.0 min
@Thickness 25.4 mm,
Temperature 31.1 °C
Gel Time 18.0 - 24.0 min
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chosun Refractories C15A Magnesia Carbon Brick for Converter
Ferrite 1, Sintered Iron-Barium Oxide Hard Magnetic Material
Chosun Refractories A-7 Insulating Firebrick
92% Alumina, opaque

PCARBC030 / 190849

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.