MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 225 GVNH BK555 Nylon 6, 25% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Availability: Asia Pacific; Europe; North America

Fillers/Reinforcement: Glass Fiber, 25% Filler by Weight

Features: Flame Retardant; Halogen Free

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Maximum Moisture Content 0.20
Linear Mold Shrinkage 0.0025 in/inISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21800 psiISO 527-2
Elongation at Break 3.5 %ISO 527-2
Flexural Strength 26800 psiISO 178
Flexural Modulus 1.25e+6 psiISO 178
Izod Impact, Notched (ISO) 3.60 ft-lb/in²
@Temperature -40.0 °C
ISO 180/1A
 5.00 ft-lb/in²
@Temperature 22.8 °C
ISO 180/1A
Charpy Impact, Notched 6.20 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 410 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 374 °FUnannealed; ISO 72-2/A
UL RTI, Electrical 149 °F
@Thickness 0.762 mm
UL 746
UL RTI, Mechanical with Impact 149 °F
@Thickness 0.762 mm
UL 746
UL RTI, Mechanical without Impact 149 °F
@Thickness 0.762 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.762 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 455 - 491 °F
Middle Barrel Temperature 455 - 509 °F
Front Barrel Temperature 455 - 518 °F
Nozzle Temperature 455 - 518 °F
Melt Temperature 428 °FPeak
 455 - 518 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0491 / 236982

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.