MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical DOVERNOX 76 Octadecyl 3,5-di-t-butyl-4-hydroxyhydrocinnamate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Dovernox 76 is a solid high molecular weight hindered phenolic antioxidant that is effective in a wide range of polymers. The low volatility provides good longterm heat aging and high temperature processing stability. It is an effective stabilizer for polyolefins, styrenics, block copolymers, elastomers, adhesives, PVC, and polyurethanes. Typical use levels range from 0.10 to 0.50%.

Information provided by DoverChem

Key Words: CAS# 2082-79-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solubility in Water 0.010 %
@Temperature 20.0 °C
Solubility >= 6000 ppm
@Temperature 20.0 °C
Methanol
 190000 ppm
@Temperature 20.0 °C
Acetone
 320000 ppm
@Temperature 20.0 °C
Hexane
 380000 ppm
@Temperature 20.0 °C
Ethyl Acetate
Molecular Weight 531 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 49.0 - 54.0 °C
 
Descriptive Properties
Physical FormWhite Free Flowing Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dover Chemical DOVERPHOS S680 Distearyl Pentaerythritol Diphosphite
PTS 30GFR-BK PBT- Flame Retardant, 30% Glass Filled PBT Black Resin
Evonik VESTOWAX® SH 105 Powder Paraffin Wax
Lithium Nitrate, LiNO3
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

WDOVER023 / 217642

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.