MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ITW Devcon® Epoxy Coat™ 7000 Non-VOC
Categories: Polymer; Thermoset; Epoxy

Material Notes: A 100% solids, 2-component, self-leveling, high impact, high abrasion floor coating with a chemical-resistant finish. Uses: Ideal floor coating for smooth or mildly spalled concrete (for high gloss finish); rebuild floors; protect floors from chemical attack. Features: Extremely durableProduces a level, high-gloss finish, High build (8-10 mils).

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 2000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 110 °FTemperature Resistance - Wet
 180 °FTemperature Resistance - Dry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 55.0 - 90.0 °FApplication Temperature
Cure Time 24.0 hour
@Temperature 24.0 °C
Foot Traffic
 24.0 hour
@Temperature 24.0 °C
Functional cure
 48.0 hour
@Temperature 24.0 °C
Full service
Pot Life 55.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Chemical/Solvent Resistance1,1,1-Trichloroethane: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Ammonia: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting oil: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric 36%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methylene Chloride: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Nitric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric 50%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 40%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
ColorLight GrayCured
Coverage400 ft²Cured. @ 8 mils
Mix Ratio by volume2.1:1
Mix Ratio by weight3.2:1
Recoat Time10 to 12 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9208 / 239717

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.