Temper: Solution Heat Treated and Cold Worked: Hard Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Hot Formed; Fair Suitability – Butt Weld Common Fabrication Processes: Bending; Cold working; Drawing; Extruding; Forging; Heading; Hot working; Impacting; Rolling; Swaging Typical uses: Pencil-type & Light Soldering Guns: Tips, Rod Extensions; Arcing and Bridging Parts; Cable; Circuit Breaker Parts; Connectors; Contacts; Electric Motor and Generator Components; Electrical Conductors Requiring Greater Strength than Copper; Electrical Connectors; Electron Tube Grid Side Rods; Parts for Electronic Devices; Semi Conductor Bases; Switch Contacts; Switch Gears; Thermal Conductors Requiring Greater Strength than Copper; Wire, High Temperature; Current Carrying Shafts and Arms; Electrode Holder Jaws; Flash Welding Electrodes; Heat Sinks; Molds; Plastic Mold Components; Resistance Welding Machine Electrodes; Seam Welding Wheels; Spot Welding Tips; Structural Parts; Wear Plates on Heavy Equipment Applicable Specifications: Bar – MILITARY MIL-C-19311; Forgings – MILITARY MIL-C-19311; Rod – MILITARY MIL-C-19311; Strip – MILITARY MIL-C-19311; Wire – Soft ASTM F9 |