38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Cast film coextrusion; heat sealing film; properties modifier for conventional films; metallizing and lamination process. Information provided by Braskem |