MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M ScotchPad™ 822 Label Protection Tape Pad
Categories: Polymer; Adhesive

Material Notes: 3M™ ScotchPad™ Label Protection Tape Pad 822 is a pre-cut pad formed with layered high-performance tape sheets featuring durable 3M™ ScotchPad™ polypropylene film backing that is strong, conformable, and resistant to impact shock, Tape sheets are coated with an aggressive adhesive to provide excellent adhesion to many types of surfaces. Each piece of tape is coupled with a liner material for easy handling and dispensing, without the need for a dispenser. Tape sheets are used for repairing broken packages, for label protection, industrial covering applications, and protection of surfaces in manufacturing processes. Tuck-in flap boxes are securely closed with these tape sheets.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3.10 milASTM D3652
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7.76 MPaLongitudinal; ASTM D3759
 15.5 MPaTransverse; ASTM D3759
Elongation at Break 160 %ASTM D3759
Peel Strength 3.4375 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypePressure sensitive hot melt rubber resin
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34152 / 168899

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.