Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping. Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass to metal seals, coaxial cables and tubes, klystrons, microwave tubes, and rectifiers. Test specimens: rod - 25mm diameter and shapes - 13mm diameter.UNS C12500, C12700, C12800, C12900, and C13000 are similar alloys having very similar mechanical properties; they are distinguished by differences in silver content. |
Fire-Refined Copper, FRTP. MIL-W-3318 |