MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Cristal™ Renew EN076-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ Renew copolyester EN076-50 is a copolyester designed to be fully compatible with the PET recycling stream. It enables recyclable cosmetics packaging with a combination of good color and high clarity for molded parts with an RIC1 resin. This product is suitable for ISBM applications and some thinner-walled molded parts for the cosmetics and personal care market. Cristal™ EN076-50 meets the definition of resin identification code #1 (RIC1) as defined by ASTM D7611. Other end-product attributes, including but not limited to size, color, auxiliary components, and availability of collection, may also impact recyclability. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Bottles-color cosmetics pkg
  • Bottles-skin care pkg
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Fragrance packaging
  • Jars-skin care pkg
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Skin care packaging

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Flexural Modulus 2350 MPaASTM D790
Izod Impact, Notched 33.0 J/m
@Temperature -40.0 °C
ASTM D256
 67.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Optical PropertiesOriginal ValueComments
Haze 0.800 %ASTM D1003
Transmission, Visible 89.0 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 277 - 293 °C
Mold Temperature 16.0 - 32.0 °C
Drying Temperature 150 °C
Dry Time 4.00 - 6.00 hour
 
Descriptive Properties
Bio-based ContentNone
Crystallization half time4.5 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4110 / 323733

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.