MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Reblend® 6520OP Unreinforced PC/ABS alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Water Absorption 0.70 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0055 - 0.0075 cm/cmSO.F.TER Method
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPaASTM D638
Tensile Strength, Yield 50.0 MPaASTM D638
Elongation at Break >= 50 %ASTM D638
Tensile Modulus 2400 MPaASTM D638
Flexural Strength 90.0 MPaASTM D790
Flexural Modulus 2600 MPaASTM D790
Izod Impact, Notched 550 J/mASTM D256/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 101 °CASTM D648
Vicat Softening Point 120 °C120°C/h at 50 N; ASTM D1525
 130 °C120°C/h at 10 N; ASTM D1525
Flammability, UL94 HB
@Thickness 0.800 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2407 MAS145 Polycarbonate
Trinseo PULSE™ 2100 LG PC/ABS Engineering Resin
Covestro Bayblend® T 45 Polycarbonate/ABS Blend
Celanese SO.F.TER Reblend® 8020OP Unreinforced PC/ABS alloy
Overview of materials for Polyphenylsulfone (PPSU)

PSOFS956 / 162420

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.