MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sandvik 22.15.3.L Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 22.15.3.L is an austenitic filler material for joining stainless steels to carbon steels or low alloy steels such as 316L to mild steel and for overlay welding where higher Mo content is desired in the second and third layers.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 180
Tensile Strength, Ultimate 600 MPa
Tensile Strength, Yield 400 MPa
@Strain 0.2 %
Elongation at Break 40 %
Reduction of Area 60 %
Charpy Impact 140 J
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 15.0 W/m-K
@Temperature 100 °C
 17.0 W/m-K
@Temperature 300 °C
 18.0 W/m-K
@Temperature 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.025 %Filler metal
 <= 0.025 %All-weld metal
Chromium, Cr 21.5 %Filler metal
 21.5 %All-weld metal
Manganese, Mn 1.5 %Filler metal
 1.6 %All-weld metal
Molybdenum, Mo 2.7 %Filler metal
 2.7 %All-weld metal
Nickel, Ni 15 %Filler metal
 15 %All-weld metal
Phosphorus, P <= 0.025 %Filler metal
 <= 0.025 %All-weld metal
Silicon, Si 0.40 %Filler metal
 0.40 %All-weld metal
Sulfur, S <= 0.015 %Filler metal
 <= 0.015 %All-weld metal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5112 / 199676

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.