MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Tivar® Premium UHMW-PE Crosslinked- Various Colors
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4200 psiASTM D638
Elongation at Break 158 %ASTM D638
Tensile Modulus 130000 psiASTM D638
Flexural Strength 3200 psiASTM D790
Flexural Modulus 108000 psiASTM D790
Compressive Strength 3000 psi
@Strain 10 %,
Temperature 22.8 °C
ASTM D695
Compressive Modulus 80000 psiASTM D695
Coefficient of Friction, Dynamic 0.15DRY VS STEEL; QTM 55007
Sand Slurry 9.01018 STEEL = 100; ASTM D4020
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Melting Point 275 °FCRYSTALLINE; ASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® MC 901 H. S. Type 6 (ASTM Product Data Sheet)
Bakelite® PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
Excelite Plastic Polycarbonate solid sheet
Mitsubishi Chemical Advanced Materials Nylatron® 101 PA66 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)

P1SMP19M / 171679

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.